This study examined the surface area and photocatalytic performance of ZnO and SnO nanoparticles (NPs), and (ZnSn)1-xMxO nanocomposites (NCs) series with M = Cu or Co and x ranging from 0.00 to 0.50. According to BET measurements, the surface area (SA) of ZnO, SnO and ZnSnO was 9.23, 6.08, and 10.55 m2/g, respectively. The SA of Cu NCs series rose from 12.55 m2/g (x = 0.10) to 33.89 m2/g (x = 0.50), whereas it increased from 11.79 m2/g (x = 0.10) to 21.61 m2/g (x = 0.50) for the Co NCs series. The higher SA in Cu-series was associated with smaller particle size and additional porosity. Photocatalytic performance was evaluated using methylene blue degradation under UV irradiation. The degradation process followed pseudo-first-order kinetics. The NCs of Cu series achieved higher efficiency than the NCs of Co series at all values of x, and the efficiency gap increased from approximately 3% at x = 0.10 to 11% at x = 0.50. After 120 minutes, the x = 0.50 of Cu series reached 84.66% degradation, while it reached 73.61% for Co-series. For comparison, ZnSnO, ZnO, and SnO gave 60.56%, 62.86%, and 55.30%, respectively. The degradation rate constant for the Cu series at x = 0.50 was 2.1 × 10-4 s⁻¹, compared to 1.8 × 10-4 s⁻¹ for Co series. The higher efficiency of Cu series than those of Co series is attributed to its narrower band gap, higher surface area, better lattice compatibility, and shallower trap states. These findings recommend using the NCs from the Cu series for wastewater purification and environmental remediation applicationsinstead of those from the Co series.